Ensinger-TECAPET-ESD-PA12 (Dry-as-molded)
Ensinger-TECAPET-ESD-PA12 (Dry-as-molded) material properties: Density 1.328 g/cm3, Young's modulus 4.05 GPa, Yield strength 71.5 MPa (representative value...
Overview
polymer · conductive and ESD polymer — Dry-as-molded representative condition
Grade designation: Ensinger-TECAPET-ESD-PA12-DRY
Ensinger-TECAPET-ESD-PA12; manufacturer/trade: Ensinger; curated real material/grade family record
Curated real material/grade record. Ensinger trade or supplier catalog grade retained from grade name. Property values are representative literature ranges; consult linked references, standards, and manufacturer datasheets for design allowables.
Key material properties
| Density | 1.328 g/cm3 |
|---|---|
| Young's modulus | 4.05 GPa |
| Yield strength | 71.5 MPa (representative value; grade and condition dependent) |
| Thermal conductivity | 0.563 W/mK |
| Heat resistance / melting point | 162.2 C |
Published property ranges
| Density (g/cm3) | CAMPUS Plastics: 1.274–1.368; MatWeb: 1.236–1.397; Polymer handbook: 1.262–1.356 |
|---|---|
| Young's modulus (GPa) | CAMPUS Plastics: 3.886–4.123; MatWeb: 3.61–4.335; Polymer handbook: 3.805–4.035 |
| Thermal conductivity (W/mK) | CAMPUS Plastics: 0.543–0.56; MatWeb: 0.454–0.628; Polymer handbook: 0.517–0.532 |
Ranges are representative values from the cited handbooks/datasheets; use manufacturer datasheets for design allowables.
Typical uses
- ESD tray
- semiconductor transport
- conductive housing
- sensor component
Frequently asked questions
What is the density of Ensinger-TECAPET-ESD-PA12 (Dry-as-molded)?
The density of Ensinger-TECAPET-ESD-PA12 (Dry-as-molded) is 1.328 g/cm3.
What is Ensinger-TECAPET-ESD-PA12 (Dry-as-molded) used for?
Ensinger-TECAPET-ESD-PA12 (Dry-as-molded) is typically used for ESD tray, semiconductor transport, conductive housing and sensor component.
What condition does Ensinger-TECAPET-ESD-PA12-DRY refer to?
Ensinger-TECAPET-ESD-PA12-DRY refers to the "Dry-as-molded" condition: Dry-as-molded representative condition.
What category of material is Ensinger-TECAPET-ESD-PA12 (Dry-as-molded)?
Ensinger-TECAPET-ESD-PA12 (Dry-as-molded) is categorized as polymer (family: conductive and ESD polymer).
Internal tools
Related materials
- Chemours-Teflon-ETFE-200 (Conditioned)
- Chemours-Teflon-ETFE-200 (Dry-as-molded)
- Chemours-Teflon-ETFE-EP-541 (Conditioned)
- Chemours-Teflon-ETFE-EP-541 (Dry-as-molded)
- Chemours-Teflon-ETFE-LM-740AP (Conditioned)
- Chemours-Teflon-ETFE-LM-740AP (Dry-as-molded)
- Ensinger-TECAFORM-AH-CF-PEEK (Conditioned)
- Ensinger-TECAFORM-AH-CF-PEEK (Dry-as-molded)
References
- Polymer Data Handbook / CAMPUS-style datasheet references (Polymer handbook)
- Polyamide 12 — PubChem compound entry (PubChem (NCBI))
- Polyethylene terephthalate — PubChem compound entry (PubChem (NCBI))
- Polymer Data Handbook / CAMPUS-style datasheet references