ASTM-A439-Class-30 (Heat treated)
ASTM-A439-Class-30 (Heat treated) material properties: Density 7.182 g/cm3, Young's modulus 146.3 GPa, Yield strength 244 MPa (representative value; grade...
Overview
metal · cast iron — Heat treated representative condition
Grade designation: ASTM-A439-Class-30-HT
ASTM-A439-Class-30; standard: ASTM; curated real material/grade family record
Curated real material/grade record. ASTM material specification/designation retained from grade name. Property values are representative literature ranges; consult linked references, standards, and manufacturer datasheets for design allowables.
Key material properties
| Density | 7.182 g/cm3 |
|---|---|
| Young's modulus | 146.3 GPa |
| Yield strength | 244 MPa (representative value; grade and condition dependent) |
| Thermal conductivity | 45.81 W/mK |
| Heat resistance / melting point | 454.7 C |
Published property ranges
| Density (g/cm3) | MatWeb: 6.89–7.399; Engineering ToolBox: 7.036–7.557; ASM/handbook: 6.83–7.334 |
|---|---|
| Young's modulus (GPa) | MatWeb: 140.453–148.99; Engineering ToolBox: 147.552–156.681; ASM/handbook: 137.53–145.824 |
| Thermal conductivity (W/mK) | MatWeb: 44.107–45.49; Engineering ToolBox: 49.248–51.059; ASM/handbook: 41.99–43.196 |
Ranges are representative values from the cited handbooks/datasheets; use manufacturer datasheets for design allowables.
Typical uses
- cast machine part
- engine block
- piping
- vibration-damped structure
Frequently asked questions
What is the density of ASTM-A439-Class-30 (Heat treated)?
The density of ASTM-A439-Class-30 (Heat treated) is 7.182 g/cm3.
What is ASTM-A439-Class-30 (Heat treated) used for?
ASTM-A439-Class-30 (Heat treated) is typically used for cast machine part, engine block, piping and vibration-damped structure.
What condition does ASTM-A439-Class-30-HT refer to?
ASTM-A439-Class-30-HT refers to the "Heat treated" condition: Heat treated representative condition.
What category of material is ASTM-A439-Class-30 (Heat treated)?
ASTM-A439-Class-30 (Heat treated) is categorized as metal (family: cast iron).
Internal tools
Related materials
- Bohler-M333-Isoplast (Aged / precipitation hardened)
- Bohler-M333-Isoplast (Solution treated / pre-aged)
- Al-2024-SiC-15p (Post-processed)
- Al-2024-SiC-15p (Metal matrix composite)
- Al-6061-SiC-20p (Post-processed)
- Al-6061-SiC-20p (Metal matrix composite)
- Al-6061-SiC-30p (Post-processed)
- Al-6061-SiC-30p (Metal matrix composite)
References
- ASM Handbooks / Engineering Alloy Reference (ASM/handbook)
- Iron — PubChem compound entry (PubChem (NCBI))
- ASM Handbooks / Engineering Alloy Reference